產品簡介 | 可鑄性耐火材料 |
本公司生產之可鑄性耐火物,具有:
|
Brand |
CA-185 |
CA-180S |
CA-180 |
CA-170 |
CA-160 |
CA-150 |
CA-140 |
CA-130 |
Properties |
||||||||
Max. Service Temp (℃) |
1800 |
1800 |
1800 |
1700 |
1600 |
1500 |
1400 |
1300 |
Bulk Density (g/cm3)
|
|
|
|
|
|
|
|
|
1400 ℃× 3hrs |
--- |
--- |
--- |
≧2.20 |
≧2.10 |
≧2.05 |
≧2.00 |
--- |
1200 ℃× 3hrs |
--- |
--- |
--- |
--- |
--- |
--- |
--- |
≧1.95 |
Cold Crushing Strength (kg/cm2) 1500 ℃× 3hrs |
≧300 |
≧280 |
≧250 |
--- |
--- |
--- |
--- |
--- |
1400 ℃× 3hrs |
--- |
--- |
--- |
≧300 |
≧300 |
≧300 |
≧250 |
--- |
1200 ℃× 3hrs |
--- |
--- |
--- |
--- |
--- |
--- |
--- |
≧150 |
Modulus of Repture (kg/cm2) |
||||||||
1500 ℃ × 3hrs |
≧80 |
≧80 |
≧60 |
--- |
--- |
--- |
--- |
--- |
1400 ℃ × 3hrs |
--- |
--- |
--- |
≧60 |
≧60 |
≧60 |
≧50 |
--- |
1200 ℃ × 3hrs |
--- |
--- |
--- |
--- |
--- |
--- |
--- |
≧15 |
Chemical Composition (%) |
≧95 |
≧90 |
≧75 |
≧60 |
≧55 |
≧45 |
≧40 |
≧35 |
Water Required (%) |
7~8 |
9~11 |
11~13 |
11~13 |
11~13 |
12~14 |
12~14 |
12~15 |
Installation Method |
Casting, Trowelling |
Brand |
CA-13I |
CA-12I |
CA-11I |
CA-10I |
CA-9I |
CA-8I |
CA-7I |
CA-6I |
CA-5I |
Properties |
|||||||||
Max. Service Temp (℃) |
1300 |
1200 |
1100 |
1000 |
900 |
800 |
700 |
600 |
500 |
Bulk Density (g/cm3)
|
≦1.4 |
≦1.3 |
≦1.2 |
≦1.1 |
≦1.0 |
≦0.9 |
≦0.8 |
≦0.7 |
≦0.6 |
Cold Crushing Strength (kg/cm2) |
≧30 |
≧30 |
≧25 |
≧25 |
≧20 |
≧15 |
≧10 |
≧10 |
≧8 |
℃× 3hrs |
1200℃ |
1200℃ |
1000℃ |
1000℃ |
800℃ |
800℃ |
600℃ |
600℃ |
500℃ |
Modulus of Repture (kg/cm2) |
≧10 |
≧10 |
≧8 |
≧8 |
≧7 |
≧6 |
≧5 |
≧5 |
≧4 |
℃ × 3hrs |
1200℃ |
1200℃ |
1000℃ |
1000℃ |
800℃ |
800℃ |
600℃ |
600℃ |
500℃ |